Raw Material | PLA Manufactured by Xinjiang Lanshan Tunhe | |
Using Machine | LDHW-600*1000 | |
Initial moisture | 9730ppm (By adding water to PLA Raw material to check how efficient the dryer can make ) Tested by German Sartorius Moisture test instrument | |
Drying Temperature set | 200℃ | |
Drying time set | 20mins | |
Final moisture | 20ppm Tested by German Sartorius Moisture test instrument | |
Final product | Dried PET Resin no clumping, no pellets sticking |
1 | Low energy consumption | Significantly lower energy consumption compared to conventional processes, through the direct introduction of infrared energy to the product Save about 40% energy consumption compared with conventional crystallizer and dryer |
2 | Minutes instead of hours | The product remains for only a few minutes in the drying process and is then available for further production steps. |
3 | Easy to clean | The drum can be opened completely,no hidden spots and can be cleaned easily with a vacuum cleaner |
4 | No clumping | Rotary drying system, its rotating speed can be increased as high as possible to get an excellent mixing of pellets. It is good in agitation, the material will not be clumped |
5 | Temperature set independently | The drum is divided into three heating zones which equipped with infrared PID temperature sensors can be set drying or crystallized temperature independently. |
6 | Siemens PLC Touch screen control | Infrared rotary dryer is designed with sophisticated temperature measurement. The material and exhaust air temperature are continuously monitored by sensors. If there is any deviations,PLC system will adjust automatically |
Recipes and process parameters can be stored in the controlling system to ensure optimal and reproducible results | ||
Easy to operate |
Heating. | Heating granules and regrind material prior to further processing (e.g. PVC, PE, PP,…) to improve throughput in the extrusion process. |
Crystallization | Crystallization of PET (Bottle flakes, granules, flakes), PET masterbatch, co-PET, PBT, PEEK, PLA, PPS, etc. |
Drying | Drying of plastic granules, and ground material (e.g. PET, PBT, ABS/PC, HDPE, LCP, PC, PP, PVB, WPC, TPE, TPU) as well as other free-flowing bulk materials. |
High-input moisture | Drying processes with high input moisture >1% |
Diverse | Heating processes for the removal of rest oligomers and volatile components. |